My SeaDek pad, which I purchased when there was a group buy on thru this board 4 or 5 years ago, is starting to delaminate. The two layers are separating from one another. Luckily, it's in small isolated locations at the sharp edges of the lettering, but it has the possibility of getting worse. I spoke with SeaDek last week and they recommended acrylic super glue to fix this. However, I'm not sure if the guy fully understood that it was the layers coming apart and the the pad from the swim deck.
I'm hesitant to use acrylic super glue as it'll harden and not be flexible. Seems like a better fix for this type of delamination would be a superglue that is flexible once cured.
Have any of you guys had this issue before, or have any thoughts?
IMG_5667.jpg
IMG_5668.jpg
mine is same age, looks similar
2006 Moomba Mobius LSV
Stereo: Kenwood KMR-D562BT
Ballast: 750 Surfside locker, 400 Surfside mid boat, 400 Gravity I, 400 Bow
Surfboards: Inland Surfer Red Woody, Triple X Composite X 58"[/SIZE]